University of Houston researchers have made a groundbreaking discovery in thermal conductivity, overturning an existing theory that boron arsenide (BAs) couldn’t compete with the heat conduction of a diamond. Instead, the team found that high-quality crystals can achieve thermal conductivity exceeding 2100 watts per meter-Kelvin (W/mK) at room temperature — possibly higher than diamond, which has been considered the best heat conductor among isotropic materials.
Published October 10th in Materials Today, this research challenges existing theories and could reshape our understanding of heat-conducting materials. It could also lead to a new semiconductor material for much better thermal management in cell phones, high-powered electronics, and data centers.
“We trust our measurement; our data is correct and that means the theory needs correction,” said Zhifeng Ren, corresponding author and a professor in the Department of Physics in UH’s College of Natural Sciences and Mathematics. “I'm not saying the theory is wrong, but an adjustment needs to be made to be consistent with the experimental data.”
The study was a collaboration between UH’s Texas Center for Superconductivity — directed by Ren — and researchers at the University of California, Santa Barbara, and Boston College.
In 2013, Boston College physicist David Broido, the study’s co-author, and others theorized that boron arsenide could rival or surpass diamond’s thermal conductivity. But according to Ren, by 2017, revised models that added four-phonon scattering — a more complex process than previously used three-phonon models — capped boron arsenide at 1360 W/mK, causing most researchers to dismiss its potential for higher thermal conductivity.
Ren and fellow researchers, however, believed that using source materials with higher purity would improve thermal conductivity because many defects existed in the samples. By purifying raw arsenic and improving synthesis techniques, the team produced cleaner crystals that showed thermal conductivity above 2100 W/mK — and with them, record-breaking thermal conductivity that exceeded theoretical expectations.
The discovery positions boron arsenide as a potential game-changer in electronics and thermal management. It not only surpasses diamond in heat conduction but also outperforms silicon — the current industry standard — as a semiconductor.
Key advantages of boron arsenide include:
- It’s easier and cheaper to manufacture than diamonds, removing the need for extreme temperatures and pressures.
- It’s not only an exceptional thermal conductor but also an effective semiconductor.
- It has the potential for better semiconducting performance than silicon due to its properties such as high thermal conductivity, wider band gap, much higher carrier mobility in both electrons and holes, and well-matched coefficient of thermal expansion.
Despite the breakthrough, the work is far from over. Texas Center for Superconductivity researchers will continue refining their materials, which they hope will push BAs’ thermal conductivity even higher. Ren invites theorists to re-examine thermal conductivity models and push beyond theoretical limits, possibly unlocking even better materials in the future.
“You shouldn’t let a theory prevent you from discovering something even bigger, and this exactly happened in this work,” Ren said.